A cedar strip canoe by Kurt Mangseth.

Readers’ Projects, Issue 53

This cedar strip canoe (top) was laminated with WEST SYSTEM® 105 Resin®/207 Special Clear Hardener®. It is the work of Kurt Mangseth of Grand Rapids, Minnesota.

Eager El catamaran Righetti Rocker

Chris Righetti of Barra de Navidad, Mexico designed and built the catamaran Eager El as well as the Righetti Rocker (both above).

waterfall table by Bill Bauer

Bay City, Michigan boatbuilder and frequent Epoxyworks contributor Bill Bauer created this whimsical waterfall table.

hockey skate repair

Chet Asher of Ocean City, New Jersey repaired the broken blade holder on his hockey skate with 105 Resin/205 Fast Hardener and 6 oz. fiberglass cloth.

The Unlimited canoe, ALALA

Alala, a 7-seat, 45′ Unlimited Canoe built by Donald Weir of Hilo, Hawaii was featured in Epoxyworks 52. Here she is under sailboard and sail with a crew of 4.