Readers’ Projects, Issue 38

This stand-up paddleboard, commonly called a SUP, was lovingly handcrafted by Joe Pakkala. His attention to detail is impressive in the herringbone inlays and the non-skid foot pads incorporated into the epoxy’s finish. As opposed to traditional adhesive non-skid pads, incorporating the nonskid into the epoxy allows you to have a safe place to stand without covering the beauty of a natural wood finish.


Scott Codding
Dave Wohl weelassie Coyote Inlay
Designed and built by veteran boat builders Gregg Hatten and Roger Fletcher, this handcrafted wooden rocking boat is a replica of the historic McKenzie Style Drift Boats that run the Big Water Rivers of the Pacific Northwest. (Does this little boat seem familiar? Maybe thats because it's a 1/3 scale version of Portola featured on the cover of Epoxyworks 35.) For more information on how to buy a rocking boat or make your own, please visit therockingboats.com