Bonding to Corian™ and Wilsonart™ Laminates

By Tom Pawlak

We recently did adhesion testing to Corian and Wilsonart surfaces with WEST SYSTEM 105 Resin and 206 Hardener at the request of a composite panel manufacturer. Corian and Wilsonart are mineral filled acrylic panels that look like granite and are often used as countertop material in kitchens and offices. Cabinetmakers and contractors typically use the panels in ½” thickness for residential applications. They are quite heavy, though not nearly as heavy as actual granite. Corian and Wilsonart are similar solid surfaces in that they can both be cut with conventional tools, then wet sanded and polished to a nice shine if they are damaged during installation. They are also available in thinner forms alone, or laminated over Continue reading