Repairing individual gelcoat blisters

Repairing Individual Gelcoat Blisters

By Tom Pawlak

Gelcoat blisters can be a serious problem if left unattended. At some point, your hull may need extensive repair, including gelcoat removal and epoxy barrier coats as described in Gelcoat Blisters: Diagnosis, Repair & Prevention. However, if you have isolated blisters and a manageable number to repair individually, we often recommend that you patch individual blisters and continue to use the boat until you determine the cause and extent of the problem. Continue reading