Hodgdon Building 124′ Cold Molded Yacht

by Mike Barker
Epoxyworks9

A Bruce King-designed 124′ sloop is taking shape* at Hodgdon Yachts, Inc. in East Boothbay, Maine. It is the largest boat ever built at Hodgdon and one of the largest wood/epoxy yachts ever built.

Even at this stage of construction she is impressive. At first glance, craftsmen fairing her keel appear to be riding the back of a breaching leviathan.

The 3″ thick cold-molded hull consists of four double-diagonal layers of 3/8″ cedar between two 3/4″ layers of mahogany laminated with WEST SYSTEM® epoxy. Fairing is nearly completed and the hull will soon be covered in two layers of biaxial cloth laminated with PRO-SET® epoxy and post cured.

After the glass skin is applied and postcured, “rolling frames” will be built over the hull to rotate it in place for installation of the 52-ton keel and finishing of the decks and interior.

The carbon composite mast will stand 172′ off the water and carry 6,761 square feet of sail. Auxiliary power will be furnished by a 550 hp Lugger diesel and a 75 hp bow thruster. She will draw 9′ 9″ with the hydraulically operated centerboard up and 26′ 6″ with it down. (Over 250 gallons of epoxy went into the glass composite centerboard trunk.) Cherry joinery will be prominent throughout the interior and the salon will feature a marble fireplace and a pipe organ.

At 350,000 pounds, the finished yacht will be too heavy to be moved on conventional tires. She’ll be skidded the several hundred yards to the launch site (cover background) on plastic runners. She will be christened ANTONISA when completed in 1999.