Protective skin creams-do they affect adhesion to the surfaces we touch?

By Tom Pawlak

We recently completed adhesion testing for a boatbuilder who was concerned about surfaces being contaminated by workers who use protective skin creams. The builder wanted to be sure that residue from the protective creams did not contaminate objects touched by workers throughout the day. We tested five products: Derma Shield™, Gloves in a Bottle™, Unique Skin™, SBS 46 Protective Cream™ and SBS 40 Medicated Skin Cream™. Continue reading