Custom Fiberglass Boat Repair

By Rich Simms, NMSC

Vessels used by the Bureau of Immigration & Customs Enforcement (ICE) can be subjected to severe conditions during law enforcement operations. Occasionally, the intense interaction between law enforcement vessel and suspect violators can result in unwanted vessel damage. The damage on this ICE interceptor was the result of intentional impact by a suspect vessel (Photos 1 and 2). Continue reading