Mold Release, PVA and Hairspray

By Tom Pawlak

PVA (polyvinyl alcohol) is a water-based liquid plastic that can be applied to waxed molds to prevent molded parts from sticking. PVA is not always required. Often laminators rely solely on mold release wax to create a surface contaminant on the mold that allows parts to be removed. However, on complicated molds and on new molds, when the risk of sticking a part in a mold is greatest, PVA can be applied over a waxed mold to minimize the chance of sticking a part.

PVA can be applied by brush, paint roller or with spray equipment. PVA often leaves a texture on the surface of the mold after it dries. This texture is duplicated or molded into the Continue reading