primer performance

House Paint Primer Performance

By Tom Pawlak

In the past, we’ve recommended applying an alkyd base primer over well cured, clean, and sanded epoxy surfaces. We wanted to know how this primer compared to the newer, fast drying primers now available. We recently did a study of various house paint primers over epoxy to support the growing number of customers using WEST SYSTEM epoxy for building restoration. Continue reading