Tag Archives: John McKibbon

Laminated Canoe

Laminated Construction Gives Lasting Value

John McKibbin recently sent pictures of his refinished 18′ canoe. He built it twenty-five years ago, using cold-molded, that is, laminated composite construction, with WEST SYSTEM® epoxy. Laminating a hull is similar to making your own plywood on a three dimensional mold. While it may take more time and effort to make a laminated hull, the results are well worth it to many. Continue reading