Tag Archives: grapnel

Grapnel

Make Your Own Grapnel

By Captain J.R. Watson

A grapnel or grappling hook is a device with curved tines or “flukes” attached to a rope used for retrieving overboard objects. For pleasure boaters, a grapnel should be small, lightweight and made of non-rusting materials. I think every cruising boat should have one. The only ones I could find were too large, or were a folding grapnel anchor, not a retrieving hook.

To get what I wanted I had to make my own. I settled on a treble configuration and chose galvanized steel. Although plenty strong, this grapnel is intended for light service, up to about 40 lb, which is about as much as the average person can lift with a line anyway. Continue reading