Producing Parts in a Matched Mold

By Captain James R. Watson

As winter wore on, I ran out of things to do. There was no snow for skiing and no ice for ice boating. I figured it was a good time to make something fancy for the new catamaran. I reckoned that fairing the compasses that stuck up out of the deck would reduce windage and make everything look cleaner. I decided to make carbon fiber compass hoods with a clear finish inside and out. This was a good application for the matched mold technique of composite construction.