G/Flex Keel Repair

By Don Gutzmer

Early in March of 2012, a local boat owner called our technical line and asked about repairing his cast iron wing keel with WEST SYSTEM® Epoxy. He asked if a technical advisor would be willing to take a look at the cracks on his keel and recommend the best way to repair it. After looking at the boat I gave the customer a call back and recommended using G/flex® Epoxy. The advantage of G/flex is that it is a toughened system that has a tensile elongation of more than 30 percent, which would prevent cracks from reappearing in the fairing compound. The boat owner then asked if I Continue reading