A Quick Fix to a Broken Spinnaker Pole

By Meade Gougeon

Adagio, our 35′ trimaran, was already off to a bad start in the 100th anniversary of the first running of the Chicago to Mackinaw race with an over-early call by the race committee. Everything went downhill from there.

Less than an hour into the race the luff wire in our number one genoa parted, putting our crucial 360 sq ft light air weapon out of business. Attempts to use it to leeward on our spinnaker pole resulted in more loads than the pole was designed to handle. It collapsed with a bang! Continue reading