Tag Archives: bottom fairing

Bottom Fairing Adagio

By Greg Bull

Most seasoned sailors would agree that a clean bottom leads to faster sailing. Sometimes it may be necessary to do more than scrub away the algae and zebra mussels, though. In the case of Adagio, 44 years of sailing was starting to ripple the bottom of the boat. Simply put, it was time to fair the bottom. While fairing the bottom of your boat may seem beyond your reach, it is a project that novices and experienced boaters alike can accomplish with a few simple tools and a love of a little manual labor. Continue reading

fairing a beach cat's bottom

Fairing a Fiberglass Beach Cat’s Bottom

By Captain James R. Watson

Dragging your catamaran over sandy beaches can abrade away material on the bottom of the hull, thereby flattening the sectional shape. Usually this area will extend 4 or 5 feet each way of the hull’s mid-section. You need to fix it so it doesn’t wear through, and to maintain optimum design performance. Continue reading