Building a Barbecue Grill Table

In midwinter, we purchased a portable barbecue and would, by summer, need some kind of table to support it. The table was to be located in an old English garden setting. We wanted a compact, all-weather structure that could be permanently affixed just off the edge of a patio, blend into the surroundings, complement a nearby picnic table, conceal a 20 lb LP gas container, and outlast a long succession of barbecue grills.

Our table design was completed by early spring. Retired Gougeon technical advisor, Brian Knight, agreed to build it as an example of high-quality, all-weather construction using treated lumber and WEST SYSTEM® epoxy. Continue reading