Tag Archives: Aluminum Boat Repair Kit

Aluminum Boat Repairs

By Greg Bull

After developing the Aluminum Boat Repair Kit we have had calls from customers saying they have a larger boat and cannot easily turn it over as recommended to work on the seams and rivets. They ask “will this kit still work on my boat?” The answer is, yes, it will. It will be a little messier but will work the same way upside down or right side up. Continue reading

New Repair Kits

New for 2012, WEST SYSTEM is offering three specialized boat repair kits designed with the do-it-yourselfer in mind. Each contains the right materials and instructions for making lasting repairs and retails for around $30 at your local stocking WEST SYSTEM dealer. Continue reading