Accelerated Testing: Hot Soak Moisture Uptake

By Bruce Niederer

We are constantly testing our products to fully understand and characterize them, and this is important both for ourselves and for our customers. A test method will usually produce results in a timely fashion, but there are times we must use an accelerated test method so we can get the results before we take that last lonely boat ride across the river Styx. This article describes some of the accelerated testing we do here.

WEST SYSTEM® epoxy is often used to provide a moisture barrier for applications that are in frequent or constant contact with water. In order to know how effective our epoxy is at resisting moisture, we have to be able to measure how much water it will Continue reading